Časovno odvisno spreminjanje akustičnih lastnosti površinsko obdelanih lesenih resonančnih plošč
ID Vadnjal May, Jakob (Author), ID Pavlič, Matjaž (Mentor) More about this mentor... This link opens in a new window, ID Straže, Aleš (Comentor)

.pdfPDF - Presentation file, Download (2,71 MB)
MD5: 6AE232B378F959B8F560BE1ED8CBFFCF

Abstract
V diplomskem delu smo spremljali časovno odvisno spreminjanje akustičnih lastnosti pri smrekovih (Picea abies (L.) Karst.) ter javorjevih (Acer pseudoplatanus (L.)) lamelah dimenzij 400 mm × 80 mm × 3 mm, premazanih s celulozno-nitratnim ali poliuretanskim premaznim sistemom. Akustične lastnosti smo proučevali z merjenjem frekvenčnega odziva ob dinamično mehanskem vzbujanju, pri prečnem nihanju. Meritve smo izvedli na neobdelanih lamelah ter po površinski obdelavi še sedemkrat, najprej štirikrat z razmikom enega tedna, nato pa še trikrat z razmikom enega meseca. Po nanosu premaznih sistemov se je značilno povečala gostota preizkušancev, prav tako pa je izrazito narastlo tudi dušenje zvoka (tanδ). Prišlo je tudi do padca lastne frekvence (f), dinamičnega modula elastičnosti (E) ter drugih akustičnih kazalnikov (ACE, RACE, Esp). Trdota celulozno-nitratnega ter poliuretanskega premaznega sistema je v postopku staranja narasla za od 50 % vse do 120 % po 1,5 meseca staranja. Časovno odvisno utrjevanje premaznih sistemov vpliva na nižanje dušenja zvoka (tanδ), kjer po 1,5 meseca dosežemo za do 50 % nižje vrednosti dušenja zvoka, ki se približujejo vrednostim površinsko neobdelanega lesa. Pri dinamičnemu modulu elastičnosti površinsko obdelanih resonančnih plošč nismo zabeležili bistvenih sprememb, le v rangu ±10 %. Zaradi časovno odvisnega zmanjšanja dušenja zvoka (tanδ) je s postopkom staranja celulozno-nitratnega ter poliuretanskega premaza prišlo do značilnega povečanja drugih akustičnih kazalnikov (ACE, RACE, K), saj je pri slednjih dušenje zvoka neodvisna spremenljivka v imenovalcu. Po 1,5 meseca staranja premazov se kazalniki stabilizirajo ter dosežejo vrednosti, ki so primerljive s površinsko nezaščitenimi lesenimi resonančnimi ploščami.

Language:Slovenian
Keywords:les, površinska obdelava, akustične lastnosti, časovna odvisnost
Work type:Bachelor thesis/paper
Typology:2.11 - Undergraduate Thesis
Organization:BF - Biotechnical Faculty
Publisher:[J. Vadnjal May]
Year:2024
PID:20.500.12556/RUL-162087 This link opens in a new window
UDC:630*829.1:812.12
COBISS.SI-ID:210002179 This link opens in a new window
Publication date in RUL:19.09.2024
Views:107
Downloads:60
Metadata:XML DC-XML DC-RDF
:
Copy citation
Share:Bookmark and Share

Secondary language

Language:English
Title:Time dependent variation of the acoustic properties of coated wood resonant panels
Abstract:
In this diploma, the change of acoustic properties over time of spruce (Picea abies (L.) Karst.) and maple (Acer pseudoplatanus (L.)) lamellae with the dimensions of 400 mm × 75 mm × 3 mm, and treated with a cellulose-nitrate or polyurethane coating, were investigated. The acoustic properties were investigated by studying the frequency response of the flexural vibration mode after dynamic-mechanical excitation of the lamellae. The tests were first conducted on untreated lamellae and repeated seven times on treated samples – four times a week apart, and three times a month apart. After the application of surface coatings, the density of the lamellae increased significantly, and the sound damping (tanδ) rose sharply. A drop in resonant frequency (f), the dynamic modulus of elasticity (E) and other acoustic properties (ACE, RACE, Esp) was also detected. In the process of ageing, the hardness of both cellulose-nitrate and polyurethane coatings rose by about 50% up to 120% in 1.5 months. The hardening process of the coatings influences sound damping (tanδ), lowering it by about 50% in 1.5 months, with measurements close to those obtained on lamellae without a surface coating. The dynamic modulus of elasticity did not change much with time, as it stayed well within the ±10% range. The reduction of sound damping (tanδ) as the coatings aged caused a rise in the other acoustic properties (ACE, RACE, K) that are directly dependent on tanδ. The aforementioned acoustic properties stabilized and reached values comparable to untreated lamellae in 1.5 months.

Keywords:wood, surface finishing, acoustic properties, time dependance