Elastocaloric effect vs fatigue life : exploring the durability limits of Ni-Ti plates under pre-strain conditions for elatocaloric coolling
ID Tušek, Jaka (Avtor), ID Žerovnik, Andrej (Avtor), ID Čebron, Matjaž (Avtor), ID Brojan, Miha (Avtor), ID Žužek, Borut (Avtor), ID Engelbrecht, Kurt (Avtor), ID Cadelli, Andrea (Avtor)

.pdfPDF - Predstavitvena datoteka, prenos (2,96 MB)
MD5: AFC9963F49231911E2E43AA472B5D10C
URLURL - Izvorni URL, za dostop obiščite https://www.sciencedirect.com/science/article/pii/S135964541830226X Povezava se odpre v novem oknu

Izvleček
Structural fatigue is the major obstacle that prevents practical applications of the elastocaloric effect (eCE) in cooling or heat-pumping devices. Here, the eCE and fatigue behaviour of Ni-Ti plates are systematically investigated in order to define the fatigue strain limit and the associated eCE. Initially, the eCE was evaluated by measuring adiabatic temperature changes at different strain amplitudes and different mean strains along the loading and unloading transformation plateaus. By comparing the eCE with and without pre-strain conditions, the advantages of cycling an elastocaloric material at the mean strain around the middle of the transformation plateau were demonstrated. In the second part of this work, we evaluated the fatigue life at the mean strain of 2.25% at the loading plateau and at the unloading plateau after initial pre-straining up to 6% and 10%, respectively. It is shown that on polished samples, durable operation of 10 5 cycles can be reached with a strain amplitude of 0.50% at the loading plateau, which corresponds to adiabatic temperature changes of approximately 5 K. At the unloading plateau (after initial pre-strain of 10%), durable operation was reached at a strain amplitude of 1.00%, corresponding to adiabatic temperature changes of approximately 8%K. The functional fatigue was analysed after the cycling and it is shown that once the sample has been stabilized there is no further degradation of the eCE, even after 10 5 cycles. These results present guidelines for the design and operation of efficient and durable elastocaloric devices in the future.

Jezik:Angleški jezik
Ključne besede:elastocaloric effect, shape memory materials, Ni-Ti, fatigue, strain
Vrsta gradiva:Članek v reviji
Tipologija:1.01 - Izvirni znanstveni članek
Organizacija:FS - Fakulteta za strojništvo
Status publikacije:Objavljeno
Različica publikacije:Recenzirani rokopis
Leto izida:2018
Št. strani:Str. 295-307
Številčenje:Vol. 150
PID:20.500.12556/RUL-127889 Povezava se odpre v novem oknu
UDK:621.56(045)
ISSN pri članku:1359-6454
DOI:10.1016/j.actamat.2018.03.032 Povezava se odpre v novem oknu
COBISS.SI-ID:15964187 Povezava se odpre v novem oknu
Datum objave v RUL:28.06.2021
Število ogledov:1581
Število prenosov:448
Metapodatki:XML DC-XML DC-RDF
:
Kopiraj citat
Objavi na:Bookmark and Share

Gradivo je del revije

Naslov:Acta materialia
Skrajšan naslov:Acta mater.
Založnik:Elsevier Science
ISSN:1359-6454
COBISS.SI-ID:16852229 Povezava se odpre v novem oknu

Licence

Licenca:CC BY-NC-ND 4.0, Creative Commons Priznanje avtorstva-Nekomercialno-Brez predelav 4.0 Mednarodna
Povezava:http://creativecommons.org/licenses/by-nc-nd/4.0/deed.sl
Opis:Najbolj omejujoča licenca Creative Commons. Uporabniki lahko prenesejo in delijo delo v nekomercialne namene in ga ne smejo uporabiti za nobene druge namene.
Začetek licenciranja:22.03.2018

Sekundarni jezik

Jezik:Slovenski jezik
Ključne besede:elastokalorični učinek, zlitine z oblikovnim spominom, Ni-Ti, utrujanje, deformacije

Projekti

Financer:ARRS - Agencija za raziskovalno dejavnost Republike Slovenije
Številka projekta:Z2-7219
Naslov:Od elastokaloričnega efekta do učinkovite hladilne naprave

Podobna dela

Podobna dela v RUL:
Podobna dela v drugih slovenskih zbirkah:

Nazaj