Sliding evolution of the mechanical behaviour of zinc dialkyldithiophosphate tribofilms on diamond-like carbon coatings
ID
Bartolomé, Luis
(
Author
),
ID
Oblak, Eva
(
Author
),
ID
Kalin, Mitjan
(
Author
)
PDF - Presentation file,
Download
(1,15 MB)
MD5: 0C5DE80BD68A14A792491528374B041F
URL - Source URL, Visit
http://link.springer.com/article/10.1007%2Fs11249-016-0666-y
Image galllery
Abstract
The evolution of the mechanical behaviour of zinc dialkyldithiophosphate (ZDDP) tribofilms on diamond-like carbon coatings during sliding contact has been studied by combining nano-indentation experimental data and finite element modelling. The nano-indentation data from the ZDDP tribofilms were obtained for two different sliding distances of the tribological tests after 15,000 and 216,000 cycles, which correspond to 25 min and 6 h, respectively. A non-homogeneous structure was found for the ZDDP tribofilms after both sliding distances, which were also verified by the local stiffness using the AFM force modulation mode. A dual structure is observed for the ZDDP tribofilms after 15,000 cycles, while three distinct components with different mechanical behaviours were found after 216,000 cycles. It was also found that the mechanical behaviour of the harder component of the ZDDP tribofilms remains almost unchanged for both sliding times, while the softer component tends to stiffen slightly over the sliding time. In addition, using the proposed algorithm with finite element simulations, the mechanical properties of the different components have been obtained, e.g. the elastic modulus E = 25.5 GPa and the yield stress Y = 1.585 GPa of the harder component for both sliding times. The softer component exhibits E = 1.65 GPa and Y = 0.144 GPa after 15,000 cycles and E = 3.5 GPa and Y = 0.17 GPa after 216,000 cycles. Finally, an intermediate component with E = 11.7 GPa and Y = 0.94 GPa has been only found at 216,000 cycles.
Language:
English
Keywords:
DLC coatings
,
ZDDP
,
finite element method
,
AFM
,
tribofilms
Work type:
Article
Typology:
1.01 - Original Scientific Article
Organization:
FS - Faculty of Mechanical Engineering
Publication status:
Published
Publication version:
Author Accepted Manuscript
Year:
2016
Number of pages:
Str. 1-9
Numbering:
Vol. 62, iss. 2
PID:
20.500.12556/RUL-106739
UDC:
539.92(045)
ISSN on article:
1023-8883
DOI:
10.1007/s11249-016-0666-y
COBISS.SI-ID:
14585883
Publication date in RUL:
14.03.2019
Views:
1252
Downloads:
715
Metadata:
Cite this work
Plain text
BibTeX
EndNote XML
EndNote/Refer
RIS
ABNT
ACM Ref
AMA
APA
Chicago 17th Author-Date
Harvard
IEEE
ISO 690
MLA
Vancouver
:
Copy citation
Share:
Record is a part of a journal
Title:
Tribology letters
Shortened title:
Tribol. lett.
Publisher:
Baltzer, Baltzer Science Publishers
ISSN:
1023-8883
COBISS.SI-ID:
2806555
Secondary language
Language:
Slovenian
Keywords:
DLC prevleke
,
metoda končnih elementov
,
tribofilmi
,
tribologija
Projects
Funder:
ARRS - Slovenian Research Agency
Project number:
P2-0231
Name:
Tribologija
Similar documents
Similar works from RUL:
Similar works from other Slovenian collections:
Back