1 - 2 / 2 ![]() ![]() ![]() ![]() |
1. Corrosion on polished and laser-textured surfaces of an Fe-Mn biodegradable alloy Matej Hočevar, Črtomir Donik, Irena Paulin, Aleksandra Kocijan, Franc Tehovnik, Jaka Burja, Peter Gregorčič, Matjaž Godec, 2017, original scientific article Keywords: Fe-Mn alloy, laser texturing, corrosion, biodegradable, EDS analyses |
2. The influence of segregation bands and hot rolling on the precipitation of secondary phases during aging at 750 °C for nickel alloy 625 Simon Malej, Jože Medved, Barbara Šetina, Franc Tehovnik, Franci Vode, Jaka Burja, Matjaž Godec, 2019, original scientific article Keywords: nickel-based superalloy, hot rolling, recrystallization, segregation, precipitation |