Effect of the shape of styrene-acrylonitrile water-filter housings on the destructive pressure, crack-initiation, propagation conditions and fracture toughness of styrene-acrylonitrile
ID Zorc, Borut (Avtor), ID Zorc, Matija (Avtor), ID Kosec, Borut (Avtor), ID Nagode, Aleš (Avtor)

.pdfPDF - Predstavitvena datoteka, prenos (5,97 MB)
MD5: ECBFA69E6DFFF1A71328E8095471F71E
URLURL - Izvorni URL, za dostop obiščite https://www.mdpi.com/2073-4360/12/2/280 Povezava se odpre v novem oknu

Izvleček
A destructive pressure test of styrene–acrylonitrile (SAN) water-filter housings showed the influence of the shape and specific details of the housings on their critical areas and their destructive pressure. The destructive pressure varies by as much as 37 bar due to different dominant stresses in the individual types of housings. In critical areas of the housings, geometrical stress concentrators generally exist. For this reason, the stress caused by the internal pressure is locally 2.75–3.4 times greater than that expected based on the water pressure, which means that cracks are initiated in these places. However, the bottom of the housings can be in a form such that the maximum stress and the crack originates in its central part without the influence of local stress concentrators. The tensile strength of the SAN is theoretically estimated at 73 N/mm$^2$, which is comparable with the literature data. The fracture toughness of the SAN is typically low, theoretically estimated in the range 1.45–3.55 MPa·m$^{1/2}$, and strongly depends on the degree of the wall’s stress-increasing rate or the crack-propagation rate. Therefore, at various crack-propagation rates, the critical crack depths are also different, in the range 100–600 µm. Due to this, the critical thickness for brittle fracture in the SAN is also different; it is ten times greater than the critical crack length. The characteristic of a sub-critical crack, i.e., the mirror zone, is its macroscopically smooth surface, which is microscopically very finely roughened. In the case of a sufficiently slowly growing sub-critical crack, the surface of the mirror zone contains characteristic parabolic markings. The over-critical, sufficiently rapidly growing cracks generally grow mainly in the plane-strain state and only the final thin layer of the remaining wall thickness breaks in the plane-stress state. The over-critical, sufficiently slowly growing cracks grow in the plane-stress state with a strong shear plastic tearing.

Jezik:Angleški jezik
Ključne besede:styrene-acrylonitrile, geometrical shape, stress concentrator, destructive pressure, fracture toughness
Vrsta gradiva:Članek v reviji
Tipologija:1.01 - Izvirni znanstveni članek
Organizacija:NTF - Naravoslovnotehniška fakulteta
Status publikacije:Objavljeno
Različica publikacije:Objavljena publikacija
Leto izida:2020
Št. strani:22 str.
Številčenje:Vol. 12, iss. 2, art. 280
PID:20.500.12556/RUL-133135 Povezava se odpre v novem oknu
UDK:669
ISSN pri članku:2073-4360
DOI:10.3390/polym12020280 Povezava se odpre v novem oknu
COBISS.SI-ID:1852511 Povezava se odpre v novem oknu
Datum objave v RUL:12.11.2021
Število ogledov:907
Število prenosov:145
Metapodatki:XML DC-XML DC-RDF
:
Kopiraj citat
Objavi na:Bookmark and Share

Gradivo je del revije

Naslov:Polymers
Skrajšan naslov:Polymers
Založnik:MDPI
ISSN:2073-4360
COBISS.SI-ID:517951257 Povezava se odpre v novem oknu

Licence

Licenca:CC BY 4.0, Creative Commons Priznanje avtorstva 4.0 Mednarodna
Povezava:http://creativecommons.org/licenses/by/4.0/deed.sl
Opis:To je standardna licenca Creative Commons, ki daje uporabnikom največ možnosti za nadaljnjo uporabo dela, pri čemer morajo navesti avtorja.
Začetek licenciranja:01.02.2020

Podobna dela

Podobna dela v RUL:
Podobna dela v drugih slovenskih zbirkah:

Nazaj